Have a question? Give us a call: +86 21 57701837

Austenitic steel ASME SA213 · TP304LN

Short Description:

The low-carbon nitrogen-strengthened chromium nickel stainless steel TP304LN is mainly used in chemical processing, power plants, and heat exchanger systems. Designed for applications requiring enhanced mechanical strength and excellent resistance to intergranular corrosion, this grade maintains superior toughness even at cryogenic temperatures. Furthermore, this grade is suitable for TIG, MAG and manual arc welding procedures.


  • Tube Grade: TP304LN, AISI 304LN, EN 1.4311, UNS S30453
  • Tube Type: Seamless
  • Tube Form: Straight, U Bend, Cut-to-Length Pieces
  • Surface Finish: Solution Annealed & Pickled (AP), Bright Annealed (BA), Polished
  • Standards (ASME/ASTM): ASME SA213, ASTM A213
  • Standards (EN): EN 10216-5
  • Product Detail

    Product Tags

    TP304LN Stainless Steel Tubes, 1.4311 Stainless Steel Tubes

    Item Specification / Details
    Stainless Steel Tube ASME SA213, ASTM A213
    Tube Size 1/8″ OD to 5″ OD (6.35 mm to 127 mm)
    Thickness Range 0.5 mm – 15 mm
    Type Seamless (无缝)
    Form Round, U Bend
    Length Single Random, Double Random & Required Length / U Bend
    End Plain End, Beveled End
    End Protection Plastic Caps
    Outside Finish 2B, BA, AP, Polished
    Delivery Condition Solution Annealed and Pickled, Bright Annealed, Cold Drawn
    Inspection, Test Reports Mill Test Certificates, EN 10204 3.1, Eddy Current Test, Hydrostatic Test
    Packing Packed in Wooden Boxes, or as per Customers Requests
    Specials Sizes and Specifications other than above can be manufactured on request

    TP 304LN . UNS S30453 . 1.4311 Chemical Composition

    Chemical Composition (in % by mass)

    Grade C (Max.) Si (Max.) Mn (Max.) P (Max.) S (Max.) Cr Ni Mo Ti N Others
    304LN 0.035 1.00 2.00 0.045 0.030 18.0 – 20.0 8.0 – 11.0 0.10 – 0.16
    1.4311 0.030 1.00 2.00 0.045 0.015 17.5 – 19.5 8.5 – 11.5 0.12 – 0.22

    TP 304LN . UNS S30453 . 1.4311 Mechanical Property

    Mechanical Property & Heat Treatment

    Grade Rp 0.2 Mpa (Min.) Rp 1.0 Mpa (Min.) Rm Mpa (Min. – Max.) A (%) (Min.) Hardness (HRB) (Max.) Heat Treatment
    304LN 205 515 35 90 Solution Annealed
    1.4311 270 300 550 – 760

  • Previous: